The short answer
Call out **carburizing** only when the drawing needs a carbon-rich case that will later be quenched and tempered. That pack is different from a through-hardening [heat-treat](https://3dwk.com/resources/when-to-specify-heat-treat-after-cnc) note, from a [nitriding](https://3dwk.com/resources/when-to-specify-nitriding-after-cnc-steel) note (a different diffusion family, usually without a carburize-and-quench cycle), and from [shot peening](https://3dwk.com/resources/when-to-specify-shot-peen-after-cnc-steel) or a [zinc, electroless-nickel, or black-oxide](https://3dwk.com/resources/zinc-plating-vs-electroless-nickel-vs-black-oxide) finish. A usable RFQ states **required or not**, the **class or standard you actually use**, **where the step sits** relative to rough machining, quench and temper, and grinding, and **which faces are masked**. A lone “carburize as needed” line is what opens a wide [quote-new.php](https://3dwk.com/quote-new.php) **rates.v1.1** estimate band—more than furnace time itself.
This page is for buyers who must package a named carburize-and-harden step on wear or contact faces of a CNC steel part. Diagrams are an **Example part** only—not a customer component or a hardness cert. Heat treat, nitriding, and peening have their own guides; this one is only about **when to write a carburizing pack**.
What carburizing after CNC steel means for quoting
The pack has to show that a carbon-diffusion case is wanted, which family or buyer document applies (gas, vacuum, or a pack/liquid class—write it only if that is what you use), how the step is ordered against machining and grinding, and which surfaces stay core-soft or masked. “Case harden for wear” is not a pack. Live Batch1 process pages used here are [CNC 3-axis Steel 1018 aerospace](https://3dwk.com/en/cnc-3axis/steel-1018/aerospace.html), [CNC 3-axis Steel 1018 tooling](https://3dwk.com/en/cnc-3axis/steel-1018/tooling.html), and [CNC 3-axis Steel 1018](https://3dwk.com/en/cnc-3axis/steel-1018.html), because those combinations already exist. Batch1 pages for 4140 combinations are not live, so the Example part is hung on the live 1018 siblings. Carburizing is still a **specified** case-hardening step, not a default on mild 1018. If the real alloy is something else, name that grade on the PDF. [When to specify 4140](https://3dwk.com/resources/when-to-specify-4140-steel-for-cnc-parts) is a material note; it does not stand in for a missing 4140 combo page.
Put the pack in the open, not inside a general notes cloud: **CARBURIZING REQUIRED; CLASS OR STANDARD CITED; AFTER ROUGH MACHINE; QUENCH AND TEMPER PER CITED CLASS; BEFORE OR AFTER GRIND AS WRITTEN; MASK THREADS AND DATUM A**. If the part should not be carburized, write **NO CARBURIZING** and, if needed, the heat-treat or other condition that does apply. File list background: [what files to send for a CNC quote](https://3dwk.com/resources/what-files-to-send-for-cnc-quote). Steel-note background: [heat treating steel after CNC](https://3dwk.com/resources/heat-treating-steel-after-cnc-machining).
When the carburizing pack is worth calling out
Write the pack when the program truly needs a carburized case plus the quench-and-temper class that follows it, and when you can point to the document you use. Leave it off a still-as-machined prototype. Do not borrow a carburizing line to stand in for nitriding, peening, or a through-hardened condition on a steel that is supposed to be hardened through the section.
If a class, a case requirement, or a customer specification exists, **put the document identifier on the PDF**. This guide does not invent a case depth, a surface or core hardness, or a 3DWK furnace recipe. Under **rates.v1.1**, the grade, the named class, masks, and sequence usually move the band more than raw material cost.
Sequence, masking, and grinding
State the order in plain language: rough machine, carburize, quench and temper to the cited class, then grind or hone any diameter that is finished after the case—or say the work enters the furnace already at a defined pre-grind size. Those two sequences are not interchangeable on an RFQ. List masked threads, datums, and faces with an explicit **MASK** note. If [MPI](https://3dwk.com/resources/when-to-specify-mpi-after-cnc-steel) is required, give it its own line; a carburizing note does not imply it.
Tolerance and inspection traps
“Carburize as needed,” “case harden” with no family or class, and a hardness or case-depth demand with no method all push the quote to **needs_manual**. A painted or as-machined 1018 bracket should get an explicit **NO CARBURIZING** pack rather than an implied wear upgrade. Related: [what needs_manual means](https://3dwk.com/resources/what-needs-manual-means-preliminary-quote).
Illustration 1 is an **Example part** Steel 1018 wear plate: carburizing required, buyer class cited, sequence after rough machine and before grind of datum A, quench and temper per that class, threads and datum A masked, remaining faces left untreated.
Example part walkthrough
**Example part:** Steel 1018 plate, two wear faces, carburizing required, buyer class or standard cited, after rough machine and before grind of datum A, quench and temper per that class, threads and datum A masked. No invented case depth, hardness number, or 3DWK recipe. With STEP plus **CARBURIZING REQUIRED; CLASS CITED; AFTER ROUGH MACHINE, BEFORE GRIND OF DATUM A; Q&T PER CLASS; MASK THREADS AND A**, [quote-new.php](https://3dwk.com/quote-new.php) can usually build a usable planning band. The same shape with only “carburize as needed for wear” often returns DFM questions or **needs_manual**. This walkthrough invents no customer order, case-depth certificate, or 3DWK-guaranteed hardness.
Illustration 2 compares a vague “carburize as needed” RFQ with a labeled class-sequence-mask pack and the tighter estimate path.
What widens bands fastest
A silent “as needed” carburize, a wear-harden note that never names the process family or the steel grade, missing masks on threads and datums, and a case-depth ask with no method. Quantity breaks do not fix an incomplete finish pack—see [how quantity breaks change CNC unit cost](https://3dwk.com/resources/how-quantity-breaks-change-cnc-unit-cost).
What to do next
Write **required or not, your class or standard, the actual steel grade, sequence versus machine / quench-and-temper / grind, and masks**, then upload the CAD on [quote-new.php](https://3dwk.com/quote-new.php). Keep carburizing off the through-harden, nitriding, and peen lines. Service pages: [CNC machining](https://3dwk.com/cnc-machining-service.php), [materials](https://3dwk.com/materials.php). **rates.v1.1** min/mid/max figures are estimates, not invoices. If the UI returns **needs_manual**, answer the carburizing-pack questions instead of forcing a number.
Common questions
Is carburizing just another name for through-hardening or for nitriding?
No. Through-hardening changes the core of a hardenable grade. Nitriding is a different surface-diffusion family and is usually packaged on its own line. Carburizing adds carbon at the surface and is then hardened to the class you cite. Write the process you actually need.
Should every wear face, or every 1018 part, be carburized?
No. Use the pack only when the program requires that case. An as-machined prototype should not inherit “carburize as needed,” and mild 1018 is not automatically a carburizing grade. If the part is an alloy, name it. Batch1 4140 combination pages are not live.
Will 3DWK fill in a default case depth?
No. Cite the standard and class on the PDF. This guide does not offer a default depth, hardness curve, or furnace recipe as a 3DWK guarantee.
How do I show grinding versus the carburizing step?
Write the order. Diameters finished after the case are not the same pack as work that is already at a defined size in the furnace. Mask any face that must stay free of case, and keep MPI, peen, and nitride notes on separate lines.